How to Build a Small Brick Wall (Non-Load Bearing)
Learn how to build a non-load-bearing brick wall in Australia. Follow our step-by-step trade guide covering concrete footings, mortar mixes, and AS 3700 standards.
Quick answer
Building a small non-load-bearing brick wall requires pouring a stable concrete strip footing at least 150mm deep, followed by laying standard 230x110x76mm masonry units in a stretcher bond. Mortar must be mixed to an M3 class (1:1:6 cement, lime, and sand) maintaining consistent 10mm joints in accordance with AS 3700.
- Skill level
- Intermediate
- Time
- 1-2 days
- Trade
- Building & Construction
- Updated
- 28 November 2026
Tools you will need
- Marshalltown 19/11D - 280mm London Pattern Brick Trowel
- Empire e70.24 - 600mm & 1200mm True Blue Box Torpedo Spirit Levels
- OX Tools Pro - 100mm Brick Bolster & Club Hammer
- Stanley FatMax - 8m Magnetic Tape Measure
- OX Tools Pro - Heavy-Duty Retractable Line & Brick Pins
- Marshalltown 81 - Half-Round Convex Brick Jointer (10mm)
What is a non-load-bearing brick wall and its typical uses in Australia?
This guide outlines the step-by-step process for constructing a small, non-load-bearing brick wall, suitable for garden borders, decorative features, or low partitions. It covers site preparation, foundation laying, bricklaying techniques, and finishing, ensuring a durable and aesthetically pleasing result for Australian homeowners and DIY enthusiasts.
What skill level is required to build a small non-load-bearing brick wall?
Intermediate — [Estimated time: 1-2 days]
What essential tools are needed for bricklaying a small wall in Australia?
Shovel: Square mouth, general digging. Spirit Level: 600mm and 1200mm for accurate levelling. Tape Measure: 8m retractable. String Line & Line Pins: For establishing straight courses. Rubber Mallet: For adjusting bricks. Brick Trowel: 280mm London pattern. Pointing Trowel: 10-12mm wide for finishing joints. Brick Hammer/Bolster & Cold Chisel: For cutting bricks. Wheelbarrow: For mixing and transporting mortar. Mortar Board/Mixing Tub: For holding mortar. Buckets: 10L for water and sand. Stiff Bristle Brush: For cleaning. Safety Glasses: AS/NZS 1337.1 compliant. Gloves: Heavy-duty work gloves. Kneepads: For comfort during bricklaying. Watering Can/Hose with fine spray: For dampening bricks and curing concrete. Angle Grinder (optional): With diamond blade for precise brick cutting.What materials are necessary for constructing a small brick wall in Australia?
Bricks: Standard common or face bricks (e.g., 230mm x 110mm x 76mm). Calculate quantity: (Wall Length (m) / 0.24) x (Wall Height (m) / 0.086) x 1.1 (for wastage). Cement: General purpose Portland cement (GP Cement). Bricklayer's Sand: Washed, sharp sand. Hydrated Lime (optional): Improves workability of mortar. Plastic Sheeting: Heavy-duty, for curing concrete. Water: Clean, potable. Reinforcing Mesh (SL62 or similar): For concrete footing (if required by local council/engineer). Timber Pegs & String: For setting out. Formwork Timber (e.g., 90x35mm treated pine): For concrete footing.Safety Requirements
Personal Protective Equipment (PPE): Always wear safety glasses, gloves, and sturdy footwear. Kneepads are highly recommended. Manual Handling: Be aware of the weight of bricks, bags of cement, and buckets of mortar. Lift with your legs, not your back. Get assistance for heavy lifting. Cutting Bricks: When using a brick hammer or bolster, wear eye protection. If using an angle grinder, ensure proper guards are in place, wear hearing protection, and a dust mask. Scaffolding: For walls exceeding 1.2m in height, proper scaffolding or a stable work platform is required. This guide focuses on low walls where scaffolding is generally not needed. Electrical Safety: If using power tools, ensure they are in good condition and connected to a Residual Current Device (RCD). Chemical Safety: Cement is an irritant. Avoid prolonged skin contact and inhalation of dust. Wash hands thoroughly after use.Step-by-Step Guide
Step 1: Site Preparation and Setting Out
Clear the area of any debris, vegetation, and loose soil. Mark out the proposed wall's footprint using timber pegs and a string line. Ensure the lines are straight and square using a builder's square or the 3-4-5 triangle method. Dig a trench for the concrete footing. For a single-skin brick wall, a trench 300mm wide and 200mm deep is generally sufficient for non-load-bearing applications, but always check local council requirements. The trench base must be firm and level.
Step 2: Formwork and Footing Preparation
Install timber formwork along the edges of the trench, ensuring it is level and securely pegged. The top of the formwork will define the top of your concrete footing. If required by local council or engineering advice, place reinforcing mesh (e.g., SL62) centrally within the trench, supported by plastic bar chairs to ensure it is embedded within the concrete. The mesh should have a minimum 25mm concrete cover on all sides.
Step 3: Pouring the Concrete Footing
Mix concrete to a general-purpose ratio of 1 part cement, 2 parts sand, and 3 parts aggregate (or use a pre-mixed bag concrete). For structural integrity, a 1:1.5:2.5 ratio is often preferred. Add water gradually until a workable consistency is achieved – not too wet, not too dry. Pour the concrete into the formwork, ensuring it fills all voids around the reinforcing mesh. Tamp the concrete with a shovel or timber offcut to remove air bubbles. Level the top surface of the concrete with a straight edge (screed board) resting on the formwork. Allow the concrete to cure for at least 3-5 days, keeping it damp and covered with plastic sheeting to prevent rapid drying and cracking. This complies with AS 3600 Concrete Structures guidelines for proper curing.
Step 4: Mixing Mortar
Once the footing is cured, prepare your mortar. For general bricklaying, a common mix ratio is 1 part cement, 1 part hydrated lime (optional, but improves workability), and 6 parts bricklayer's sand. If not using lime, a 1 part cement to 4 parts sand mix is also common. Mix dry ingredients thoroughly, then gradually add water until a plastic, workable consistency is achieved – it should hold its shape on the trowel without being too stiff or too runny. Mix only what you can use within 1-2 hours.
Step 5: Laying the First Course (Bed Course)
Lay a bed of mortar approximately 10-15mm thick along the length of the footing. Use your trowel to create a furrow in the centre of the mortar bed. Lay the first brick at one end, gently tapping it into position with a rubber mallet to ensure it's level and aligned with your string line. Apply mortar to the end of the next brick (known as "buttering the perp end") before laying it against the first, maintaining a consistent 10mm joint. Continue laying bricks, checking for level and alignment frequently with your spirit level and string line. Ensure all perp (vertical) joints are filled.
Step 6: Laying Subsequent Courses (Stretcher Bond)
For a strong, aesthetically pleasing wall, use a stretcher bond pattern where each brick in a course overlaps the bricks below by half its length. Start the second course with a half brick (cut with a brick hammer/bolster or angle grinder) to create the offset. Lay a bed of mortar, butter the perp ends, and lay bricks, maintaining consistent 10mm bed (horizontal) and perp (vertical) joints. Continuously check for level, plumb (vertical alignment), and straightness using your spirit level and string line. Build up the corners first (known as "leading up"), typically 3-4 courses high, then fill in the middle sections.
Step 7: Jointing and Finishing
As you lay each course, or once a section of wall is complete, finish the mortar joints. This can be done with a pointing trowel or a jointing tool. A concave or weathered joint is common and helps shed water. Rake out any excess mortar from the joints before they fully set. Once the mortar has stiffened but is not fully hard, use a stiff brush to clean off any mortar smears from the brick faces. Avoid cleaning too early as it can smear the mortar, and too late makes it very difficult to remove.
Step 8: Curing and Final Clean-up
Keep the newly laid brickwork damp for at least 3-5 days, especially in hot or windy conditions, by lightly misting it with water. This aids in the proper curing of the mortar, increasing its strength and durability. Once the mortar is fully cured (typically 7-10 days), perform a final clean-up, removing any remaining mortar splashes or debris.
Common Mistakes to Avoid
Pro Tips
Dampen Bricks: In hot weather, lightly dampen bricks before laying to prevent them from absorbing water too quickly from the mortar, which can weaken the bond. Use a Gauge Rod: Create a timber rod marked with the height of each course (brick height + mortar joint, e.g., 76mm + 10mm = 86mm) to ensure consistent course heights. Keep Tools Clean: Regularly clean your trowels and other tools to prevent mortar build-up, which can affect their performance and accuracy. Work in Sections: For longer walls, work in manageable sections, completing the laying and jointing before moving to the next. Practice Dry Laying: Before mixing mortar, dry lay a few courses of bricks to get a feel for the pattern and spacing.Recommended Tools
Ox Tools Pro Brick Trowel (London Pattern): Known for its balance and durability, making mortar spreading easier. Spear & Jackson Fibreglass Handle Rubber Mallet: Durable and effective for gentle brick adjustments without damage. Stanley FatMax Xtreme Spirit Level (1200mm): High accuracy and robust construction for reliable levelling. Makita 230mm Angle Grinder (with diamond blade): For efficient and precise cutting of bricks, especially for half bricks or intricate cuts. Husqvarna K 770 Power Cutter (for larger projects): If you anticipate many cuts or thicker materials, hiring a dedicated power cutter can save significant time and effort.Frequently asked questions
- What is the standard mortar mix ratio for a non-load-bearing brick wall?
- The standard mortar mix ratio for a non-load-bearing garden or decorative brick wall is 1 part cement, 1 part hydrated lime, and 6 parts brickies sand (M3 classification under AS 3700). Adding a plasticiser improves workability, ensuring durable, weather-resistant 10mm bed and perp joints across all courses.
- How deep does a concrete footing need to be for a low brick wall?
- A non-load-bearing brick wall up to 1 metre high typically requires a concrete footing between 150mm and 200mm deep, and at least 300mm wide (twice the wall width). Footings must rest on firm, undisturbed soil or compacted road base, reinforced with trench mesh (such as SL72) to prevent ground movement cracking.
- How many bricks per square metre do I need in Australia?
- Standard Australian brickwork requires approximately 48.5 bricks per square metre for a single-skin (half-brick) wall. Bricks measure 230mm long by 110mm wide by 76mm high. When planning a project, allow for standard 10mm mortar joints and always order an extra 5% to 10% to cover cuts, offcuts, and breakages.
- What Australian standards apply to domestic bricklaying?
- Domestic brickwork in Australia is governed by AS 3700:2018 (Masonry Structures) and the National Construction Code (NCC). Brick units must comply with AS/NZS 4455.1, while built-in components like wall ties and damp-proof courses must meet AS/NZS 2699 standards. Low garden walls under 1 metre generally do not require council engineering approval unless retaining soil.
- How do you prevent a small, freestanding brick wall from falling over?
- Prevent stability failure by keeping the wall height within safe height-to-thickness ratios (maximum 800mm to 1000mm high for a single 110mm skin) and incorporating attached piers every 1.8 to 2.4 metres. For added stability, bed galvanized brick-tie reinforcing mesh into horizontal joints every third or fourth course.
- How long should mortar cure before striking joints or applying loads?
- Tool or strike mortar joints with a jointer once the mix is thumbprint hard, typically 30 to 60 minutes after laying depending on humidity and brick suction. Allow the completed brickwork to cure undisturbed for at least 24 to 48 hours before exposing to rain, and a full 28 days to achieve maximum compressive strength.
Written by Bricko, the Building & Construction specialist at VIC.Tools.