Tools you will need

  • Trojan - Brick bolster chisel (75mm)
  • Stanley - FatMax AntiVibe Brick Hammer (57-500)
  • Bunnings - General Purpose Cement (20kg bag)
  • Everbuild - Hydrated Lime (20kg bag)
  • Whites Woven Products - Washed Brickies Sand (20kg bag)
  • Nylex - 9L Bucket
  • Marshalltown - Margin Trowel (50 x 125mm)
  • Estwing - Cold Chisel (25mm)
  • Craftright - Spirit Level (600mm)
  • Ozito - Cordless Blower (PXBBL-018)

🧱 How to Fix Loose Bricks in a Wall

What causes loose bricks in an Australian wall?

Loose bricks in an older wall are usually caused by failed mortar, water entry, movement, or corrosion of nearby steel such as lintels. A small localised repair is often suitable for a careful DIYer, but if the wall is load-bearing, bulging, badly cracked, or has multiple loose areas, you should get a licensed bricklayer and possibly a structural engineer involved in line with AS 3700 Masonry Structures.

This guide covers how to remove and relay one or a few loose bricks, make the area watertight again, and match the surrounding mortar as closely as possible.

What skill level is required to fix loose bricks in Australia?

Intermediate β€” Estimated time: 2–4 hours for 1–3 bricks, plus 24–48 hours curing time

What tools are required to fix loose bricks in Australia?

Brick bolster and club hammer for removing old mortar and lifting bricks
Pointing trowel and brick trowel for placing and finishing mortar
Joint raker or old screwdriver for cleaning out joints to 15–20 mm
Stiff masonry brush and hand broom for dust removal
Bucket or mixing tub, minimum 20 L
Margin trowel or small mixer for mortar mixing
Spray bottle or sponge for dampening bricks and joints
Spirit level, minimum 600 mm
Tape measure
Cold chisel for careful trimming if required
Caulking gun if using masonry repair adhesive in very minor non-structural repairs
Ladder or mobile scaffold if working above safe reach height
PPE: safety glasses, gloves, P2 dust mask, hearing protection, steel-cap boots

What materials are needed for brick repair in Australia?

Matching replacement bricks if existing bricks are cracked or damaged
Brickies mortar mix or mortar ingredients:
General repair mortar: 1 part cement : 1 part lime : 5–6 parts brickies sand
Clean water, approximately 2–5 L
Brickies sand, if mixing your own mortar
Plastic sheet or damp hessian for curing
Masonry sealant only if required around adjacent penetrations or flashings, not as a substitute for mortar
Oxide tint if needed to colour-match existing mortar
Small wedges or timber packers for temporary support if needed during relaying

Safety Requirements

Wear safety glasses, gloves, a P2 dust mask, long sleeves, and steel-cap boots.
Mortar dust and brick dust can contain silica. Avoid dry sweeping where possible and damp down dusty material.
Use correct lifting technique. Bricks and mortar buckets are heavier than they look.
If working above ground level, use a stable platform. For higher work, compliant scaffolding is safer than stretching from a ladder.
Do not remove bricks from a wall that appears to be load-bearing and unstable without professional advice.
If you see bulging brickwork, major stair-step cracking, rusted lintels, or movement around doors/windows, stop and seek professional assessment. Structural repairs may require engineering certification and compliance with local council and state requirements.
If the repair is near a wet area or wall penetration prone to moisture, ensure any waterproofing detail complies with AS 3740 where applicable.

Step-by-Step Guide

Step 1: 1️⃣ Check whether the repair is DIY-safe

Start by checking how serious the problem is.

A DIY repair is generally suitable where:

only 1–3 bricks are loose
the wall face is still straight
there are no major cracks wider than about 3 mm
the bricks themselves are mostly sound
the loose area is not supporting a lintel, beam, or heavy load

Do not proceed as DIY if:

the wall is bulging
several courses are loose
there are stepped cracks through many bricks
the wall is retaining soil
the loose bricks are under a window lintel or above a large opening
the wall is a boundary or structural wall with visible movement

In those cases, call a bricklayer or engineer. AS 3700 is the key Australian Standard for masonry performance.

Step 2: 2️⃣ Remove the loose brick and old mortar

If the brick is already loose, lift it out carefully by hand. If it is only partially loose, use a brick bolster and hammer to break out the surrounding failed mortar first.

Work slowly to avoid damaging nearby bricks.

Remove all old mortar from:

the cavity or opening in the wall
the sides of adjoining bricks
the top and bottom bed joints
the loose brick if you are reusing it

Aim to clean back to solid material and rake out joints to at least 15–20 mm depth. If the brick cracks during removal, replace it with a matching brick rather than trying to glue it back together.

Step 3: 3️⃣ Inspect the cause before relaying

Before putting the brick back, work out why it came loose.

Common causes include:

mortar deterioration from age
repeated wetting and drying
minor settlement
vibration
rusting steel lintels pushing the brickwork
salts and moisture damage

If the surrounding mortar is soft and powdery, rake out any loose material around the affected area as well.

If you notice rust stains above windows or doors, or cracks radiating from corners, there may be a lintel issue that needs professional repair before relaying bricks.

Step 4: 4️⃣ Clean and dampen the brick and opening

Brush all dust and loose particles out of the opening with a stiff masonry brush.

Then lightly dampen:

the replacement brick
the sides of the opening
the bed joint surfaces

Do not soak the wall so it is dripping wet. The goal is a damp surface that stops the old brick and surrounding masonry from sucking moisture out of the fresh mortar too quickly.

This step is especially important in hot or windy Australian conditions.

Step 5: 5️⃣ Mix a suitable repair mortar

For most older brick home repairs, use a workable bricklaying mortar rather than a strong concrete mix.

A good general mortar for brick repairs is:

1 part cement : 1 part lime : 5–6 parts brickies sand

If you are using a premixed brickies mortar, follow the bag instructions and only add enough water to achieve a firm, buttery consistency.

Avoid making the mortar too wet. Sloppy mortar weakens the bond, stains brick faces, and can slump out of the joints.

For very old homes with softer bricks and lime-rich mortar, a softer mortar is often better than a hard high-cement mix. Mortar should usually be weaker than the brick so the wall can move and breathe without damaging the masonry units.

Step 6: 6️⃣ Butter the joints and relay the brick

Using a pointing trowel, place a full bed of mortar at the bottom of the opening, usually about 10 mm thick.

Butter mortar onto:

both side joints of the brick
the top or back contact areas if needed for a tight fit

Slide the brick into position carefully and press it into place so mortar squeezes evenly from the joints.

Check the brick:

sits flush with adjacent bricks
follows the existing bond line
has even joint widths, typically around 10 mm
is level and aligned with the wall face

Use the spirit level and your eye line along the course. Remove or add a little mortar as needed to get the brick sitting true.

Step 7: 7️⃣ Tool the joints to match the existing wall

Once the mortar has started to firm up slightly, tool the joints to match the original profile.

Common joint finishes include:

ironed/concave
flush
struck
weathered

For most brick veneer homes, a neat ironed joint gives good weather resistance.

Compact the mortar well into the joints, then clean off excess with the trowel. Lightly brush the area only after the mortar has started to stiffen. Brushing too early can smear mortar across the brick face.

Step 8: 8️⃣ Clean the brick face properly

Use a damp sponge sparingly to remove small smears from the brick face.

Do not flood the wall with water and do not use acid cleaners on fresh mortar.

If some mortar residue remains, let it harden and clean it gently later. Overcleaning fresh joints often causes more damage than leaving a light haze temporarily.

Step 9: 9️⃣ Cure the repair

Fresh mortar needs time to gain strength.

Protect the repair from:

direct hot sun
strong wind
heavy rain

In warm weather, lightly mist the area over the next 24 hours if it is drying too fast. Cover with plastic sheeting or damp hessian if needed, without pressing against the joints.

Allow at least 24–48 hours before the area is exposed to heavy weather, vibration, or washing.

Step 10: πŸ”Ÿ Check for water entry and ongoing movement

After curing, inspect the wall again.

Make sure:

the joints are fully filled
there are no visible gaps
the brick is firm when pressed
there are no fresh cracks forming nearby

If the brick loosens again or cracks reopen, the issue is likely movement or moisture-related rather than just failed mortar. At that point, a more thorough inspection is needed.

Common Mistakes to Avoid

1.Repointing or relaying over loose, dusty mortar instead of cleaning back to sound material first.
2.Using mortar that is too strong for older bricks, which can trap moisture and damage the brick face over time.
3.Setting the brick dry without dampening it, causing the mortar to dry too fast and lose bond.
4.Making the mortar too wet, which leads to sagging joints and weak repairs.
5.Ignoring signs of structural movement such as bulging, stepped cracks, or movement above openings.
6.Smearing mortar over the brick face and trying to wipe it off too early, which stains the wall and weakens the joint finish.
7.Attempting repairs from an unsafe ladder position instead of using proper access equipment.

Pro Tips

πŸ’‘ Take one of the loose bricks or a clear photo to a masonry supplier to get the closest match in size, colour, and texture.
πŸ’‘ If only the mortar has failed and the brick is sound, clean and reuse the original brick for the best visual match.
πŸ’‘ Older Australian homes often used softer mortar. Matching hardness matters just as much as matching colour.
πŸ’‘ Do a small mortar colour test first and let it dry, because mortar almost always dries lighter than it looks when wet.
πŸ’‘ For very small non-structural hairline joint repairs, a mortar repair cartridge can be faster, but it is not a replacement for properly relaying a loose brick.
πŸ’‘ If you need a large mixer, scaffold, or demolition hammer for a bigger job, hire is usually more economical than buying for one-off repairs.

Recommended Tools

Brick bolster and 1.8–2.2 kg club hammer β€” for controlled mortar removal and brick lifting
Pointing trowel 150 mm β€” ideal for packing mortar into tight joints
Spirit level 600 mm β€” for checking brick alignment and face plumb
Jointing tool/brick jointer β€” for matching existing concave or ironed joints
Stiff masonry hand brush β€” for cleaning joints without damaging brick faces

Frequently asked questions

What causes bricks to become loose in an Australian wall?
Loose bricks in an Australian wall are typically caused by deteriorated mortar due to age, water penetration from faulty flashing or drainage, structural movement, or corrosion of embedded steel components like lintels. These factors compromise the mortar's integrity, leading to instability and potential structural issues if not addressed promptly.
When should I call a professional bricklayer for loose bricks?
You should call a professional bricklayer if the wall is load-bearing, exhibits significant bulging or extensive cracking, or has multiple areas of loose bricks, as these indicate potential structural compromise. Adhering to AS 3700 Masonry Structures, a licensed professional can assess the full extent of damage and ensure safe, compliant repairs.
What type of mortar should I use for repairing loose bricks in Australia?
For repairing loose bricks, use a mortar mix that matches the strength and composition of the existing mortar, typically a weaker mix for older structures to prevent damage to the bricks. For most repairs, a M3 or M4 mortar mix (e.g., Cement Australia GP Cement with hydrated lime and washed sand) is suitable, ensuring it complies with AS 3700.
How do I prepare the area before re-laying a loose brick?
Before re-laying a loose brick, thoroughly remove all old, loose mortar from the brick and the surrounding joint using a cold chisel and stiff brush, then dampen the area. This ensures optimal adhesion for the new mortar and prevents premature drying, which is crucial for a durable repair according to best practice.
What are the common mistakes to avoid when fixing loose bricks?
Common mistakes include failing to clean out old mortar thoroughly, using mortar that is too strong for older bricks, neglecting to dampen the bricks and joints, making the mortar too wet, and ignoring proper curing procedures. These errors can lead to poor bond, premature failure, and further damage to the masonry.
How long does it take for mortar to cure properly in Australian conditions?
Mortar typically requires 24-48 hours to achieve initial set, but full curing can take 28 days, depending on environmental factors like temperature and humidity in Australian conditions. Proper curing involves keeping the mortar damp for the first few days to ensure maximum strength and durability, as outlined in AS 3700 guidelines.

Written by Bricko, the Building & Construction specialist at VIC.Tools.