How to repair crumbling mortar in brickwork

Learn how to repair crumbling mortar in brickwork across Australia. Follow our step-by-step guide to rake out joints, mix compatible mortar, and repoint.

Quick answer

Repairing crumbling mortar involves raking out damaged joints to a minimum depth of 15 mm using a plugging chisel. The joint must be cleared of dust, dampened, and refilled with a 1:1:6 cement, lime, and sand mortar mix complying with AS 3700. Tool the finished profile to ensure weatherproofing.

Skill level
Intermediate
Time
4–8 hours for a small wall area of 2–5 m², or 1–2 days for larger sections
Trade
Building & Construction
Updated
28 November 2026

Tools you will need

  • Trojan 12mm - Plugging Chisel
  • Stanley FatMax 1.4kg - Anti-Vibe Club Hammer
  • Marshalltown 6mm x 150mm - Tuck Pointer Trowel
  • OX Tools Pro 250mm - Philadelphia Brick Trowel
  • Fuller 10mm x 12mm - Half-Round Iron Jointing Tool
  • Sabco Professional - Stiff Polypropylene Joint Brush
  • Nylex 2L - Multipurpose Pressure Pump Sprayer
  • Makita 125mm 18V LXT - Angle Grinder with Dust Extraction Shroud

What is involved in repairing crumbling mortar in Australian brickwork?

Repairing crumbling mortar in brickwork is usually a repointing job: removing loose or failed mortar from the joints and replacing it with fresh, compatible mortar. For many older Australian homes, this is a practical DIY maintenance task that improves weather resistance and appearance, but widespread cracking, bulging walls, or loose bricks can indicate structural issues that should be assessed by a licensed bricklayer or engineer in line with AS 3700 Masonry Structures.

What skill level is required for repairing crumbling mortar in brickwork?

Intermediate — Estimated time: 4–8 hours for a small wall area of 2–5 m², or 1–2 days for larger sections

What tools are required to repoint crumbling mortar in Australian brickwork?

Plugging chisel, 10–12 mm wide, for raking out mortar by hand
Club hammer, 1–1.5 kg, for controlled removal of loose mortar
Tuck pointer or pointing trowel, 6 mm, 10 mm and 12 mm sizes, to suit joint widths
Brick trowel, 250–280 mm, for loading mortar
Jointing tool / brick jointer, half-round or square profile, to match existing finish
Stiff nylon or natural fibre brush for cleaning joints
Bucket, 20 L, or mixing tub for mortar mixing
Drill with mixing paddle or hand mixing hoe for small batches
Spray bottle or hand sprayer for dampening joints
Sponge and clean rags for tidy-up
Margin trowel or small scraper for tight areas
100–125 mm angle grinder with mortar rake and dust shroud for experienced users only
Shop vacuum or M-class dust extractor if using power tools
Ladder rated to AS/NZS 1892 or mobile scaffold for higher work areas
Drop sheets or plastic to protect paving, windows and garden beds

What materials are needed for repointing brickwork in Australia?

Mortar or repointing mix matched to the existing mortar colour and hardness
For many standard brick homes: 1 part GP cement : 1 part hydrated lime : 5.5–6 parts clean brickies sand
For older soft bricks or heritage work: use a softer, more lime-rich compatible mortar and seek specialist advice before proceeding
Clean brickies sand, washed and well graded
GP cement
Hydrated lime
Clean water
Mortar colour oxide, if needed for colour matching
Masking tape and plastic sheeting for protecting adjacent finishes
Replacement bricks, if any bricks are cracked, spalled or loose
Premixed repointing mortar as an alternative to site mixing for small DIY jobs
Approximate mortar quantity: allow 5–10 kg of dry mix per m² of face brickwork where joints are raked out to 15–20 mm depth, depending on joint width and brick size

Safety Requirements

Wear safety glasses, P2 respirator, hearing protection, gloves, long sleeves and steel-cap boots
Mortar dust and brick dust can contain respirable crystalline silica; control dust with hand tools where possible, or use a grinder fitted with dust extraction
Do not overreach from a ladder; use a properly set ladder or hire a mobile scaffold for extended work or areas above about 2 m
Isolate the work area below to prevent injury from falling debris
Use safe manual handling when lifting cement, sand and scaffold components
Avoid repointing in rain, on saturated walls, in strong wind, below 5°C, above 35°C, or where frost is likely overnight
If the wall shows bulging, stepped cracking, movement around openings, or loose structural brickwork, stop work and get a licensed bricklayer or engineer; structural repairs may require engineering certification and council approval
If the home is heritage-listed or in a heritage overlay, check council requirements before altering mortar appearance or joint profile

Step-by-Step Guide

Step 1: Assess the brickwork and confirm it is suitable for DIY repair

Check whether the issue is limited to surface mortar failure or whether there are larger structural problems. Crumbling mortar, shallow gaps and localised weathering are usually suitable for repointing. If you find stepped cracks, bowed walls, loose sections, rusted lintels, large gaps wider than about 5 mm, or bricks moving when pressed, the wall may need professional attention rather than a simple mortar repair.

Look closely at:

Joint width, usually around 10 mm in standard face brickwork
How deep the mortar has failed
Whether the existing mortar is hard cement-based or softer lime-rich mortar
The joint profile, such as flush, ironed, raked or weather-struck

For older Australian homes, matching the original mortar hardness is important. Mortar should generally be softer than the brick so it can absorb movement and weathering without damaging the brick faces.

Step 2: Choose a suitable day and prepare the work area

Pick a cool, dry day with no rain forecast for at least 24 hours. Winter is often a good time for this work, but avoid very cold mornings, heavy dew, fog, or frost-prone conditions.

Prepare the area by:

Moving outdoor furniture and pot plants clear
Laying drop sheets over paving and garden beds
Taping off aluminium frames, painted surfaces and nearby finishes
Setting up safe access with a stable ladder or mobile scaffold

If the repair area is more than a small patch, working in sections of about 0.5–1 m² at a time is easier and gives better control over finish and curing.

Step 3: Rake out the failed mortar

Remove all loose, cracked and friable mortar from the joints. The aim is to create a clean, solid recess for the new mortar to bond to.

Rake out the joints to:

A minimum depth of 15 mm
Or about 2 times the joint width, whichever is greater

Use a plugging chisel and club hammer for best control, especially on older bricks. Work carefully to avoid chipping the brick arrises, which are the sharp visible edges of the bricks.

If using an angle grinder:

Only use it on straight joints
Fit a mortar rake blade and dust shroud
Keep the cut centred in the joint
Avoid vertical perps unless you are very confident, as they are easy to overcut

Do not remove more material than necessary. The goal is sound, square-edged joints, not enlarged gaps.

Step 4: Clean out all dust and loose material

Brush out the raked joints thoroughly with a stiff brush. Vacuum the joints if needed. Any dust left behind can weaken the bond of the new mortar.

The joints should be:

Clean
Firm at the back and sides
Free of loose mortar crumbs
Free of paint, moss, salt build-up or oily residue

If there is heavy efflorescence or moss, remove it before repointing. Do not acid wash the wall immediately before repointing, as residue can affect adhesion and fresh mortar.

Step 5: Dampen the brickwork

Before applying new mortar, lightly dampen the joints and surrounding brick faces with a spray bottle or hand sprayer. The surface should be damp, not dripping wet.

This is especially important in:

Warm weather
Windy conditions
Dry, absorbent older bricks

Pre-dampening stops the dry brickwork from sucking moisture out of the fresh mortar too quickly, which can lead to weak, powdery joints and poor curing.

Step 6: Mix a compatible mortar

For general repointing on many standard brick homes, a suitable site mix is:

1 part GP cement
1 part hydrated lime
5.5–6 parts clean brickies sand

Add clean water gradually until the mortar is workable and holds on the trowel without slumping. It should be firm enough to pack into joints, not wet and sloppy.

Important notes:

Match the existing mortar colour and texture as closely as possible
Do not use a very hard, high-cement mortar on old soft bricks
For older Federation, Victorian or heritage brickwork, a softer lime-rich mortar may be required
Mix small batches that can be used within about 30–45 minutes

A premixed repointing mortar is often the easiest option for beginners and gives more consistent colour from batch to batch.

Step 7: Pack the new mortar into the joints

Using a tuck pointer or small pointing trowel, press the mortar firmly into the joint in layers. Start with the vertical joints, then do the horizontal joints.

For deeper joints:

Pack in one layer first
Let it firm slightly
Add a second layer if needed

Make sure the mortar is fully compacted to the back of the joint with no voids. This is critical for durability and water resistance.

Do not smear large amounts over the brick face. Work neatly and keep the repair area small enough to finish before the mortar skins over.

Step 8: Tool the joints to match the existing finish

Allow the mortar to firm up until it is thumbprint hard, then tool the joint to match the original profile.

Common joint finishes include:

Flush joint
Ironed / concave joint
Weather-struck joint
Slightly recessed joint

For most face brickwork exposed to weather, a compacted ironed or slightly weathered finish performs better than a rough, open-textured finish.

Tooling does two things:

Improves appearance
Compresses the surface of the mortar to increase weather resistance

Avoid tooling too early, as the mortar will drag and smear. Avoid tooling too late, as it will crumble and not compact properly.

Step 9: Clean the brick faces carefully

Once the mortar has started to firm, brush the brick faces lightly with a soft or medium brush to remove crumbs and smears. Use a damp sponge only sparingly.

Do not:

Flood the wall with water
Scrub aggressively
Use acid cleaner on fresh mortar

Fresh mortar can stain face bricks if overworked. Gentle, minimal cleaning at the right time gives the best result.

Step 10: Cure and protect the repair

New mortar needs controlled curing to develop strength and reduce shrinkage cracking.

For the next 2–3 days:

Protect the wall from rain and direct hot sun
Lightly mist the repaired area if conditions are dry or windy
Keep children and pets away from the work area
Avoid pressure washing or harsh cleaning

In winter, curing is slower. In hot weather, it may need more frequent misting and shading. Do not allow the joints to dry out too rapidly.

Step 11: Inspect the finished work

After curing, inspect the joints for:

Hairline shrinkage cracks
Gaps at the edges of bricks
Hollow or underfilled sections
Colour mismatch
Smears left on brick faces

Minor touch-ups can usually be done with the same mortar mix. If large areas continue to fail, or mortar keeps cracking or falling out, there may be moisture ingress, movement, or incompatible mortar underneath that needs professional diagnosis.

Common Mistakes to Avoid

1.Using mortar that is too hard for the existing brickwork, which can cause brick faces to crack or spall over time.
2.Raking out joints too shallowly; new mortar needs at least 15 mm depth or it may not bond properly.
3.Repointing over dusty or dry joints without cleaning and dampening first.
4.Making the mortar too wet, which weakens the mix and increases shrinkage.
5.Trying to repair structural cracks or loose brickwork as a cosmetic DIY job instead of getting professional advice.

Pro Tips

Test your mortar colour on a small, hidden area first. Mortar often dries lighter than it looks when wet.
For older homes, softer mortar is usually safer than a strong cement-rich mix. The mortar should weather before the bricks do.
Work on small areas, especially as a beginner. A 0.5 m² section is easier to clean and finish neatly.
Match the joint profile as well as the colour. Even well-matched mortar can look wrong if the finish is different.
If you need access equipment for a one-off job, hiring a mobile scaffold is usually far more economical than buying, and much safer than stretching off a ladder all day.

Recommended Tools

OX Pro Plugging Chisel, 10 mm or 12 mm — good control for hand-raking mortar without damaging brick edges
Marshalltown Tuck Pointer Set — useful for matching common 6 mm, 10 mm and 12 mm joint widths
Makita 125 mm Angle Grinder with dust shroud — suitable for experienced DIY users tackling longer horizontal joints
Ragni or OX brick jointer / jointing tool — helps create a consistent concave or flush finish
Bailey Pro ladder or hired aluminium mobile scaffold — safer access for external walls and upper sections

Frequently asked questions

What is the best mortar mix ratio for repointing brickwork in Australia?
The best mortar mix for repointing standard modern Australian brickwork is a 1:1:6 ratio, consisting of one part general purpose cement, one part hydrated building lime, and six parts washed brickies sand. Older heritage brickwork requires a softer mix, such as 1:2:9, or a non-hydraulic lime-putty mortar to prevent the brick faces from spalling.
How deep should crumbling mortar be raked out before repointing?
Crumbling mortar joints must be raked out to a minimum depth of 15 mm, or roughly twice the thickness of the joint, whichever is greater. Raking out to this depth creates a square-edged profile inside the joint. This ensures adequate mechanical keying and prevents the new mortar layer from delaminating under thermal stress.
Can I use straight cement to fix crumbling mortar joints?
No, straight Portland cement or strong Class M4 mortar should never be used to repair crumbling brick joints. Modern cement cures harder than most clay bricks, trapping moisture and forcing thermal movement into the masonry units. This causes permanent spalling, face cracking, and structural failure contrary to AS 3700 masonry principles.
Why does mortar crumble in Australian homes?
Mortar crumbles primarily due to rising damp, salt damp, prolonged weather exposure, or poor original mixing ratios containing insufficient lime. In coastal Australian areas, airborne salts crystallise inside porous mortar joints (subflorescence), causing the binder to break down mechanically and revert to loose sand over time.
Do I need to wet brick joints before repointing?
Yes, joints must be thoroughly cleaned of dust and misted with clean water using a pump sprayer immediately before applying new mortar. Dry masonry units rapidly pull moisture out of fresh mortar via capillary action, preventing the cementitious binder from fully hydrating, which results in weak, powdery, and unbonded joints.
When is crumbling mortar a sign of structural failure?
Crumbling mortar indicates structural failure when accompanied by stepped diagonal cracking through bricks, bulging wall sections, dropping lintels, or shearing damp-proof courses. If cracks exceed 5 mm or bricks are loose, halt work and consult a licensed structural engineer or registered builder under the National Construction Code guidelines.

Written by Bricko, the Building & Construction specialist at VIC.Tools.