How to Repair Mortar Joints in Brickwork
Learn how to repair mortar joints in brickwork. Repointing stops water ingress and spalling by replacing cracked mortar to AS 3700 masonry standards.
Quick answer
Repairing mortar joints in brickwork involves raking out degraded mortar to a minimum depth of 15 mm, dampening the joint, and packing fresh cement-lime mortar securely into the gap. Matching mortar strength to the existing brick is essential under Australian Standard AS 3700 to prevent brick spalling and moisture ingress.
- Skill level
- Intermediate
- Time
- 4–8 hours per 5 m² of brickwork, plus 2–7 days curing time
- Trade
- Building & Construction
- Updated
- 28 November 2026
Tools you will need
- Makita GA5040RZ - 125 mm Angle Grinder with Dust Extraction Shroud
- Kango 8 mm x 200 mm - Diamond Mortar Raking Blade
- Estwing 570 g (20 oz) - Club Hammer with Shock Reduction Grip
- Footprint 225 mm - Plugging Chisel
- Marshalltown 150 mm x 10 mm - Brick Jointer / Tuck Pointer
- Ox Pro Heavy Duty - Aluminium Mortar Hawk (300 mm x 300 mm)
- Hozelock 1.25 L - Multi-Spray Pressure Mister Bottle
- Tradeware 100 L - Heavy Duty Steel Brickies Wheelbarrow
What is involved in repairing mortar joints in brickwork?
Repairing mortar joints, also called repointing, restores the weather resistance and appearance of brickwork by removing loose or cracked mortar and replacing it with fresh mortar matched to the original joint. For older Australian homes, this is a practical maintenance job that helps stop water ingress, reduce brick damage, and extend the life of the wall.
What skill level is required for repairing mortar joints?
Intermediate — Estimated time: 4–8 hours per 5 m² of brickwork, plus 2–7 days curing time
What tools are required for repointing brickwork?
What materials are needed for mortar joint repairs?
Typical mortar options:
Approximate quantities:
Safety Requirements
Step-by-Step Guide
Step 1: Inspect the brickwork and confirm the repair scope
Walk the wall and identify which joints are cracked, recessed, powdery, or missing mortar. Tap the mortar lightly with a plugging chisel; loose mortar will sound hollow and break away easily. Also inspect the bricks themselves for spalling, movement, and salt attack.
If you see any of the following, stop and get professional advice:
As a DIY rule, repointing is suitable for aesthetic defects and localised weathered joints, not for structural wall movement.
Step 2: Match the existing mortar before you start
The replacement mortar should be slightly softer than the brick, not harder. On many older Australian homes, a hard cement-rich mortar can damage soft clay bricks by trapping moisture and forcing the brick face to break down.
Check:
For a small patch, prepare 2–3 test mixes on a spare brick or inconspicuous area. Let them dry for 24–48 hours, because mortar usually dries lighter than when first placed.
Step 3: Prepare the work area
Cover paths, windows, garden beds, and painted surfaces with plastic sheeting. Remove any vines, dirt, cobwebs, or loose surface contamination. If the wall has been painted or sealed, repointing results may be inconsistent unless coatings are removed first.
Set up:
Only work on a manageable section, typically 1–2 m² at a time.
Step 4: Remove damaged mortar to the correct depth
Rake out defective mortar to a minimum depth of 15–20 mm, or about 2 to 2.5 times the width of the joint, whichever is greater. Remove all loose, crumbly, and cracked mortar until you reach sound material.
Best method by wall type:
Important technique:
Clean out all debris as you go.
Step 5: Brush and wash the joints clean
Use a stiff masonry brush to remove all dust and loose particles from the raked joints. Then lightly rinse or spray the wall so the joints are clean but not saturated.
Mortar will not bond properly to dusty joints. Fine dust left behind can cause the new mortar to debond or crack early.
Step 6: Pre-dampen the brickwork
Before repointing, dampen the brick faces and joints with a spray bottle or low-pressure sprayer. The bricks should be cool and slightly damp, with no standing water.
This step is critical in Australia’s warm and dry conditions. Dry bricks can suck moisture out of fresh mortar too quickly, leading to:
In hot weather, you may need to re-dampen the area several times.
Step 7: Mix the mortar correctly
Mix only small batches that can be used within 30–45 minutes. A suitable general repointing mix for many non-heritage brick homes is:
Add water slowly until the mortar is firm, workable, and able to stay on the pointing trowel. It should not be wet or sloppy. For patch repairs, pre-blended repointing mortar can be more consistent and easier for DIY use.
Important:
Let the mixed mortar sit for 5–10 minutes, then remix briefly before use.
Step 8: Pack the vertical joints first
Using a small pointing trowel, mortar gun, or hawk and jointer, firmly press mortar into the vertical perp joints first. Work the mortar in layers if the joint is deeper than 15 mm, ensuring there are no voids behind the face.
Compact the mortar tightly. The goal is a fully filled joint, not just a thin surface skim.
Finish the mortar slightly proud of the brick face at first.
Step 9: Fill the horizontal bed joints
After the perp joints, fill the horizontal bed joints. Again, press the mortar firmly into the back of the joint, then build it out to the face.
For wide or deep joints:
Only repoint as much area as you can tool before the mortar stiffens.
Step 10: Tool the joints to match the existing profile
Once the mortar has started to firm up and is thumbprint hard, tool the joints to the same finish as the original wall. Common profiles include:
Tooling compresses the mortar face and improves durability. Avoid tooling too early, as this drags mortar out of the joint. Avoid tooling too late, as the mortar will crumble and not compact properly.
Step 11: Brush off the wall and tidy the brick faces
When the mortar has firmed further, lightly brush the joints and brick faces with a soft brush to remove crumbs and create a neat finish. Do not use excessive water or acid cleaners on fresh mortar.
If mortar smears remain on the brick face:
Acid cleaning is not recommended for fresh DIY repointing and can damage both the mortar and some brick types.
Step 12: Cure the mortar properly
Fresh mortar needs slow curing to gain strength and reduce shrinkage. Lightly mist the repaired area for the next 2–3 days in warm or windy weather. Protect it from direct sun, strong wind, and rain with hessian or breathable sheeting if needed.
Good curing practice:
Mortar colour will continue to change as it cures.
Step 13: Inspect the finished work
After 24–48 hours, check the joints for:
Touch up small defects promptly while the colour difference is still manageable. If large areas are mismatched, it is usually better to redo a full panel rather than isolated patches.
Common Mistakes to Avoid
Pro Tips
Recommended Tools
Frequently asked questions
- How deep do you need to grind out mortar joints before repointing?
- Mortar joints must be raked out to a minimum depth of 15 mm to 20 mm, or roughly twice the joint width. Raking to a solid, square profile ensures the fresh mortar locks mechanically into the joint. Removing insufficient depth prevents adequate adhesion and leads to early bond failure and cracking.
- What mix ratio should be used for repointing brick mortar in Australia?
- Modern Australian brickwork generally uses an M3 mortar mix of 1 part cement, 1 part hydrated lime, and 6 parts washed brickies sand. Older homes built before 1950 require a softer, lime-rich mix such as 1 part lime to 3 parts sand to prevent damage to softer clay bricks.
- Can you use an angle grinder to remove old mortar from brick joints?
- Yes, a 125 mm angle grinder fitted with a diamond mortar-raking blade and dust extraction shroud is standard. However, you must avoid nicking the brick arrises. Hand chisels, such as plugging chisels, should always be used near corners, perpendicular perpends, and on historic or heritage masonry.
- Why is it important to wet brick joints before applying new mortar?
- Dry clay bricks act like sponges, rapidly drawing water out of fresh mortar before the cement can properly hydrate. Misting the cleaned joints with water prevents flash drying, avoids shrinkage cracking, and ensures the mortar cures to full compressive strength in accordance with Australian masonry construction standards.
- What is the difference between repointing and tuckpointing?
- Repointing is the structural replacement of deteriorated mortar joints flush with or slightly recessed into the brick edge. Tuckpointing is a specialist decorative finish where the joint is filled with mortar matching the brick colour, followed by a narrow, contrasting ribbon of lime putty applied precisely down the centre.
- How long does repointed mortar take to cure in Australian conditions?
- Repointed mortar achieves initial set within 24 to 48 hours, but requires up to 28 days for full compressive curing. Keep fresh joints sheltered from direct sun and wind, lightly misting them daily for the first three days to manage heat-induced shrinkage, especially in warmer Australian climates.
Written by Bricko, the Building & Construction specialist at VIC.Tools.