Repointing a brick wall means removing damaged or loose mortar joints and replacing them with fresh mortar to restore strength, weather resistance, and appearance. It’s a common maintenance job on older Australian brick homes, especially where mortar has cracked, turned sandy, or started allowing mo

Skill level
Intermediate
Time
1–2 days for a small wall section of around 5–10 m²
Trade
Building & Construction
Updated
28 November 2026

Tools you will need

  • Brick bolster and club hammer for removing loose mortar
  • Pointing trowel, preferably 6 mm and 10 mm
  • Mortar hawk or small hand board
  • Stiff
  • Bucket or mixing tub, minimum 20 L
  • Drill with paddle mixer for mortar mixing
  • Brick jointer or pointing iron to suit joint profile
  • Spray bottle or garden sprayer for dampening brickwork
  • Sponge and clean water bucket for light clean
  • Ladder or compliant scaffold platform for elevated work

🧱 How to Repoint a Brick Wall — DIY Trade Guide for Australian Homes

What is involved in repointing a brick wall?

Repointing a brick wall means removing damaged or loose mortar joints and replacing them with fresh mortar to restore strength, weather resistance, and appearance. It’s a common maintenance job on older Australian brick homes, especially where mortar has cracked, turned sandy, or started allowing moisture into the wall.

Done properly, repointing can extend the life of the brickwork and improve presentation, but the key is using the right mortar mix, joint depth, and finishing method. For heritage homes or structural cracking, get advice from a bricklayer or engineer before starting.

What skill level is required for repointing a brick wall?

Intermediate — Estimated time: 1–2 days for a small wall section of around 5–10 m²

What tools are required for repointing a brick wall?

Brick bolster and club hammer for removing loose mortar
Joint raker or angle grinder with mortar raking blade for controlled joint removal
Pointing trowel, preferably 6 mm and 10 mm
Mortar hawk or small hand board
Stiff-bristle brush and soft hand brush
Bucket or mixing tub, minimum 20 L
Drill with paddle mixer for mortar mixing
Brick jointer or pointing iron to suit joint profile
Spray bottle or garden sprayer for dampening brickwork
Sponge and clean water bucket for light clean-up
Ladder or compliant scaffold platform for elevated work
Drop sheets to protect paving and garden areas

What materials are needed for repointing a brick wall?

Pre-blended mortar mix or separate cement, hydrated lime, and washed brick sand
Mortar colouring oxide if matching existing joints
Clean potable water
Masking tape and plastic sheeting for nearby finishes if required
Mild brick cleaning solution if final clean-down is needed
Test sample board or scrap timber for mortar colour trial
For general repointing, a typical site mix may be around 1:1:6 cement:lime:sand for older brickwork, depending on wall type and brick hardness
Avoid overly hard mortar on older homes; mortar should generally be softer than the brick
For related concrete work, common mix ratios are 1:2:3 general purpose and 1:1.5:2.5 structural, but these are not typically used for repointing mortar

Safety Requirements

Wear safety glasses, dust mask or P2 respirator, gloves, long sleeves, and hearing protection when grinding or raking joints
Silica dust from mortar removal is hazardous; use dust control and avoid dry cutting where possible
Use safe manual handling when lifting bags of mortar or moving scaffold components
If working above ground level, use properly erected scaffolding or a stable work platform rather than overreaching from a ladder
Check for electrical cables, meter boxes, and pipe penetrations before grinding
Structural cracking, bulging walls, or movement may require assessment by a qualified engineer or licensed contractor
Repointing does not replace structural repair; masonry work should align with AS 3700 where relevant, and structural matters may require engineering certification
If the wall adjoins wet areas or penetrations, waterproofing works must comply with AS 3740 where applicable

Step-by-Step Guide

Step 1: Inspect the wall and confirm repointing is suitable

Check whether the wall has surface mortar deterioration only, or whether there are deeper structural issues. Repointing is suitable where mortar joints are cracked, recessed, loose, sandy, or allowing minor moisture entry.

If the bricks themselves are badly spalled, the wall is bulging, or cracks run through multiple courses in a stepped pattern, repointing alone may not solve the problem. Heritage homes may also need a softer lime-rich mortar to avoid damaging older bricks.

Look at the existing joint profile as well. Most suburban homes use flush, ironed, or slightly recessed joints. Matching the original finish makes the repair less visible.

Step 2: Test the existing mortar and choose the right new mix

The new mortar should be compatible with the existing brickwork. On older homes, especially pre-1970s walls, avoid a very hard high-cement mix because it can trap moisture and cause the bricks to fail before the mortar does.

A softer mix is generally preferred for older clay bricks. For many Australian repair jobs, a mortar in the range of 1:1:6 cement:lime:sand is a common starting point, but matching the original mortar is more important than using a one-size-fits-all recipe.

Do a small sample patch in an inconspicuous spot and let it dry properly before proceeding. Mortar usually dries lighter than it looks when wet.

💡 Test both colour and texture. Using local washed sand often has a bigger effect on the final look than oxide colour alone.

Step 3: Remove the failed mortar to the correct depth

Rake out the old mortar carefully to a minimum depth of around 15 mm or about 2 to 2.5 times the width of the joint, whichever is greater. Remove all loose and powdery material until you reach sound mortar.

Use a joint raker for small jobs or an angle grinder with care for larger areas. Do the horizontal bed joints first, then the vertical perpends. Avoid widening the joints or chipping the brick arrises.

Take your time around soft or heritage bricks, as they damage easily. If the brick edges start breaking away, switch to hand tools rather than power tools.

Step 4: Clean out dust and dampen the wall

Brush out all joints thoroughly so no dust or loose grit remains. A stiff-bristle brush works well, and compressed air can help if available, though brushing is usually enough for DIY work.

Lightly dampen the joints and surrounding brick faces before applying new mortar. The wall should be damp, not dripping wet. This stops dry bricks from sucking moisture too quickly out of the fresh mortar.

In hot or windy Australian conditions, you may need to mist the wall more than once. Good moisture control helps prevent weak, crumbly joints and poor bond.

Step 5: Mix the mortar

Mix only small batches you can use within about 30–45 minutes, depending on weather. Use clean water and mix until the mortar is workable and firm enough to stay on the trowel without slumping.

The mortar should be plastic, not runny. If it is too wet, it will smear the brick face and shrink excessively as it cures. If it is too dry, it will not bond properly into the joint.

Use the same measured mix for the entire wall section to keep the colour consistent. A drill and paddle mixer gives a more even batch than hand mixing.

Step 6: Pack the new mortar into the joints

Using a pointing trowel and hawk, press mortar firmly into the joints in layers if needed. Deep joints should be filled in multiple passes rather than one thick application.

Do the vertical joints first, then the horizontal joints, or follow a consistent pattern that lets you compact the mortar properly. The important part is full compaction with no hidden voids.

Push the mortar right to the back of the raked-out joint. Surface smearing alone is not repointing and will fail quickly.

Step 7: Tool and finish the joints to match the existing profile

Allow the mortar to firm up until it is thumbprint hard, then tool it to the required finish. Common finishes include flush, ironed, weathered, or slightly recessed.

Use a jointer or pointing iron sized to the joint, often around 10 mm. Tooling compresses the surface, improves weather resistance, and gives a neat finished appearance.

Brush off crumbs once the mortar has started to set, but do not scrub too early or you will drag mortar from the joints and stain the brick face.

Step 8: Cure the mortar properly

Fresh mortar needs slow curing, especially in warm, dry, or windy weather. Lightly mist the repointed area over the next 24–72 hours as needed to prevent rapid drying.

Protect the wall from direct sun, strong wind, and heavy rain. Plastic sheeting can help, but keep it off the wall face so condensation does not stain the work.

Proper curing is one of the biggest differences between a durable job and a crumbly one. Do not rush this stage.

Step 9: Final clean-up and inspection

Once the mortar has cured enough, inspect the wall for missed spots, pinholes, or inconsistent joint finish. Touch up small defects while the work is still green enough to blend.

Clean any light mortar haze gently with a dry or barely damp brush. Avoid aggressive acid washing on fresh mortar, especially on older bricks, as it can damage both the joint and brick face.

Stand back and view the wall in different light. Good repointing should blend with the existing work rather than look patched and obvious.

Common Mistakes to Avoid

1.Removing only the surface mortar and not raking back to at least 15 mm of sound material
2.Using mortar that is too hard for older bricks, which can lead to brick spalling and trapped moisture
3.Repointing onto dusty, dry joints without dampening first, causing poor bond
4.Making the mix too wet, which leads to shrinkage, staining, and weak joints
5.Cleaning too early or too aggressively and dragging mortar out of the joints

Pro Tips

💡 Repoint a test area first, especially if colour matching old suburban or heritage brickwork
💡 Work on small sections at a time, around 1–2 m², so you can tool the joints at the right set
💡 In hot weather, start early and keep the wall shaded to improve curing
💡 Match the original joint style exactly; even good mortar work looks wrong if the profile does not suit the house
💡 For large areas, hiring a mortar rake grinder and small scaffold is usually more economical than buying if this is a one-off repair job

Recommended Tools

Mortar raking angle grinder blade — faster removal of old joints on larger areas
Pointing trowel set 6 mm / 10 mm — better control in narrow and standard joints
Brick jointer or pointing iron — essential for matching existing joint profile
Paddle mixer for drill — gives consistent mortar batches and colour
Mobile scaffold hire — safer and more efficient than ladder work for extended wall sections

Frequently asked questions

What is involved in repoint a brick wall?
Repointing a brick wall means removing damaged or loose mortar joints and replacing them with fresh mortar to restore strength, weather resistance, and appearance. It’s a common maintenance job on older Australian brick homes, especially where mortar has cracked, turned sandy, or started allowing mo
What skill level do I need for repoint a brick wall?
Intermediate — Estimated time: 1–2 days for a small wall section of around 5–10 m²
What are common mistakes when repoint a brick wall?
1. Removing only the surface mortar and not raking back to at least 15 mm of sound material 2. Using mortar that is too hard for older bricks, which can lead to brick spalling and trapped moisture 3. Repointing onto dusty, dry joints without dampening first, causing poor bond 4. Making the mix too wet, which leads to shrinkage, staining, and weak joints 5. Cleaning too early or too agg
What tools do I need for repoint a brick wall?
This guide includes a comprehensive tools list. Key building & construction tools are detailed in the Tools Required section.
What is the best mortar mix for repointing older Australian brickwork?
For older Australian brickwork, a softer mortar mix is generally recommended to prevent damage to the bricks. A common mix is 1:1:6 (cement:lime:sand) or even 1:2:9 for very soft bricks, as advised by heritage masonry experts. The goal is for the mortar to be weaker than the brick, allowing it to fail before the brick does.
How deep should I rake out mortar joints when repointing?
Mortar joints should be raked out to a minimum depth of 15-20mm, or until sound mortar is reached, whichever is greater. According to AS 3700:2018, this ensures sufficient depth for the new mortar to bond effectively and provide structural integrity, preventing premature failure of the repointing work.
What safety precautions should I take when repointing a brick wall?
When repointing, always wear appropriate Personal Protective Equipment (PPE) including safety glasses, gloves, and a dust mask, especially when raking out old mortar. According to SafeWork Australia guidelines, ensure stable access with ladders or scaffolding, and be mindful of dust control to prevent respiratory issues. Use hearing protection if operating power tools.