Tools you will need
- Brick bolster and club hammer for careful mortar removal
- Plugging chisel or joint raker for hand raking joints
- Mortar hawk or hand board
- Stiff nylon brush and masonry brush
- Spray bottle or garden sprayer for dampening brickwork
- Bucket or mixing tub
- Paddle mixer or drill with mixing attachment
- Jointing tool or iron to suit existing joint profile
- Sponge and clean rags for final clean
- Ladder or mobile scaffold if working above shoulder height
🧱 How to Repoint Brickwork: A Practical DIY Guide for Australian Homes
What is involved in repointing brickwork in Australia?
Repointing brickwork means removing loose or weathered mortar from the joints and replacing it with fresh mortar to improve weather resistance, durability, and appearance. For Australian homeowners, it’s a common repair on older brick homes where cracked or missing joints can allow water ingress, salt attack, and further brick deterioration.
Done properly, repointing can extend the life of your wall, but the key is using the right mortar, raking out to the correct depth, and avoiding damage to the bricks. For loadbearing walls, major cracking, or heritage homes, professional advice may be needed, and any structural concerns should be assessed in line with AS 3700 Masonry Structures.
What skill level is required for brick repointing?
Intermediate — Estimated time: 1–2 days for a small wall section of around 5–10 m²
What tools are essential for repointing brickwork?
What materials are needed for a brick repointing project?
Suggested mortar options by volume:
Use the softer mix that matches the existing mortar as closely as possible. The new mortar should generally be no harder than the original mortar or surrounding brick.
Safety Requirements
Step-by-Step Guide
Step 1: Inspect the wall and identify the cause
1️⃣ Check whether repointing is the right repair
Look for mortar that is crumbly, recessed, cracked, loose, or missing from the joints. Tap suspicious areas with a pointing tool and check whether the mortar powders easily or falls out.
Also inspect for underlying issues such as leaking gutters, rising damp, failed flashings, salt staining, or movement cracks. Repointing will not solve active movement or water coming from another source.
If the wall is loadbearing and has major cracking, bulging, or separation, seek professional advice before starting. Structural masonry must comply with AS 3700.
Step 2: Match the existing mortar
2️⃣ Choose the correct mortar strength, colour, and texture
This is one of the most important parts of the job. Older Australian homes often used softer lime-rich mortars, especially before modern cement-rich mixes became common. If you use a mortar that is too hard, moisture can become trapped and the bricks may start to crack or spall.
Break out a small sample of the old mortar and compare:
Mix a small test batch and allow it to dry before committing to the full job. Mortar always dries lighter than it looks when wet.
💡 For soft older bricks, a lime-containing mortar is usually safer and easier to work than a strong cement-heavy mix.
Step 3: Prepare the work area
3️⃣ Set up access, protection, and dust control
Lay down drop sheets and cover nearby windows, paving, air-conditioning units, and garden beds. If working higher than about 1.8 m, a mobile scaffold is often safer and more efficient than repeated ladder moves.
If using an angle grinder, fit a dust shroud and connect it to a suitable extractor. For small repairs, hand raking is slower but gives better control and reduces the risk of chipping brick edges.
Lightly clean the wall so you can clearly see the joints and the extent of damage.
Step 4: Rake out the old mortar
4️⃣ Remove defective mortar to the correct depth
Rake out the mortar to a depth of at least 15 mm, or around 2 to 2.5 times the width of the joint, whichever is greater. The aim is to remove all loose and weak material so the new mortar has enough depth to bond properly.
Use:
Do not widen the joints unnecessarily, and do not chip the brick faces. Any damaged brick edges will remain visible after the repair and can make the wall look patchy.
Brush out all dust and loose debris once raking is complete.
Step 5: Clean and pre-wet the joints
5️⃣ Prepare the masonry for new mortar
Thoroughly brush and vacuum the joints. Any dust left behind can weaken the bond.
Then lightly dampen the joints and brick edges with a spray bottle or garden sprayer. The wall should be damp but not dripping. This helps prevent the dry masonry from sucking moisture out of the new mortar too quickly.
In hot or windy Australian conditions, this step is critical. If the mortar dries too fast, it can shrink, crack, or fail to bond properly.
Step 6: Mix the mortar
6️⃣ Mix small batches to a workable consistency
Mix the mortar to suit the existing wall and only prepare as much as you can use in about 30–45 minutes. The ideal consistency is firm enough to stay on the trowel, but plastic enough to pack tightly into the joints.
As a general guide:
Add water slowly. Avoid overly wet mortar, as it will smear more easily, shrink more, and can weaken the finished joint.
If colour matching matters, keep your measuring consistent from batch to batch. Use the same bucket or scoop every time.
💡 Pre-blended repointing mortars can save time and improve colour consistency, especially for DIYers doing visible front elevations.
Step 7: Pack the joints in layers
7️⃣ Fill the joints firmly and completely
Load the mortar onto a hawk and use a pointing trowel or tuck pointer to press it deeply into the joints. Start with the horizontal bed joints, then complete the vertical perpend joints.
For deeper joints, fill in layers of about 10 mm rather than trying to pack it all in at once. Compact each layer well to eliminate voids.
Make sure the mortar fully contacts the back and sides of the joint. Gaps behind the face can allow water entry and lead to early failure.
Work in manageable areas of roughly 0.5–1 m² at a time so you can finish the joints before the mortar firms up too much.
Step 8: Tool the joints to match the existing profile
8️⃣ Finish the joints for weather resistance and appearance
Once the mortar becomes thumbprint firm, tool the joints to match the original profile. Common joint finishes include:
For most external walls, a compacted bucket-handle style joint performs well because it sheds water and compresses the mortar surface.
Do not tool too early or the mortar will drag and smear. Do not leave it too late or it will be difficult to compact properly.
After tooling, lightly brush the joints to remove loose crumbs and blend the finish.
Step 9: Cure the mortar properly
9️⃣ Control drying for strength and durability
Fresh pointing needs slow, even curing. Protect the area from direct sun, strong wind, and rain for at least 24–72 hours, depending on weather.
Lightly mist the wall if conditions are hot or dry, especially during the first 24 hours. This is particularly helpful with lime-containing mortars.
Avoid pressure washing or aggressive cleaning immediately after repointing. Let the mortar cure first.
Step 10: Final clean-up and inspection
🔟 Check the finish and touch up small defects
Once the mortar has firmed up, clean the brick faces with a dry or slightly damp sponge. Avoid flooding the wall. If minor smears remain, allow the mortar to cure before attempting any further cleaning.
Stand back and inspect:
Touch up any small voids while the work is still green enough to bond.
If acid-based brick cleaning is being considered, use extreme caution and only where suitable for the brick type and mortar. Poor use of acid can stain or damage the wall.
Common Mistakes to Avoid
Pro Tips
💡 On heritage-style homes, mortar joint style matters just as much as colour. Matching the original profile can make repairs almost disappear.
💡 If the wall shows white salt deposits, fix the moisture source first. Repointing alone will not stop recurring efflorescence.
💡 Keep a separate bucket of clean water and a sponge just for brick-face clean-up. Dirty water quickly causes staining.
Recommended Tools
Frequently asked questions
- What is involved in repoint brickwork?
- Repointing brickwork means removing loose or weathered mortar from the joints and replacing it with fresh mortar to improve weather resistance, durability, and appearance. For Australian homeowners, it’s a common repair on older brick homes where cracked or missing joints can allow water ingress, sa
- What skill level do I need for repoint brickwork?
- Intermediate — Estimated time: 1–2 days for a small wall section of around 5–10 m²
- What are common mistakes when repoint brickwork?
- 1. Using mortar that is too hard for older bricks, which can cause brick faces to crack or spall over time. 2. Raking out too shallowly. New mortar needs a minimum depth of around 15 mm to bond and perform properly. 3. Grinding carelessly and chipping brick edges, especially on softer older clay bricks. 4. Repointing without dampening the joints first, causing the new mortar to dry too fast
- What tools do I need for repoint brickwork?
- This guide includes a comprehensive tools list. Key building & construction tools are detailed in the Tools Required section.
- What is the Australian standard for masonry structures?
- The Australian standard for masonry structures is AS 3700 Masonry Structures. This standard outlines requirements for the design and construction of masonry, including brickwork, ensuring structural integrity and durability. It is crucial for tradies to consult this standard, especially when dealing with loadbearing walls or significant structural repairs.
- How deep should mortar joints be raked out for repointing?
- Mortar joints should be raked out to a minimum depth of 15-20 mm, or at least twice the joint width, to ensure adequate bonding and durability of the new mortar. According to best practice, this depth allows for proper keying and prevents premature failure of the repointing work, especially in Australian weather conditions.
- What PPE is recommended for brick repointing in Australia?
- Recommended PPE for brick repointing in Australia includes safety glasses (AS/NZS 1337.1), hearing protection (AS/NZS 1270), and a P2-rated respirator (AS/NZS 1716) to protect against silica dust. According to SafeWork Australia guidelines, gloves and sturdy work boots are also essential for hand and foot protection during the process.
Written by Bricko, the Building & Construction specialist at VIC.Tools.