Skip to main content

How to weld galvanised steel safely on site

Weld galvanised steel safely on site by grinding back coatings, using PAPR respirators and ensuring ventilation to prevent zinc oxide fume exposure per AS/NZS 1554.

Quick answer

Welding galvanised steel safely requires grinding the zinc coating back at least 50mm from the weld line, using a PAPR respirator meeting AS/NZS 1716, and ensuring local exhaust ventilation. Structural welds must comply with AS/NZS 1554. These controls prevent metal fume fever and weld porosity caused by zinc oxide fumes.

Skill level
Intermediate
Time
1–4 hours depending on access, quantity of welds, surface prep and ventilation setup
Trade
Welding & Fabrication
Updated
29 November 2026

Tools you will need

  • Lincoln Electric Weldanpower 180 - MIG/GMAW Welder
  • ESAB Rebel EMP 215ic - Multi-Process Welder
  • 3M Versaflo TR-315 - PAPR Welding Respirator
  • Makita GA9020 - 230mm Angle Grinder
  • Honeywell North 7700 - Half Face Respirator (backup)
  • Weldclass Platinum - Welding Gauntlet Gloves
  • Trotec TAF 20 - Portable Fume Extractor
  • Esko Steel Blue - Flame-Resistant Welding Jacket

🔥 Safe On-Site Welding of Galvanised Steel — Fume Control, Prep and Compliant PPE Guide

Why is welding galvanised steel on site hazardous?

Welding galvanised steel on site creates significant hazards due to zinc oxide fumes, contaminated weld zones and increased risk of poor weld quality if the coating is not correctly removed. For Australian trade professionals, the job must be approached with strict PPE, ventilation, hot work controls and disciplined weld preparation to protect personnel and achieve sound welds.

This guide covers safe on-site procedures for fabricators, fence installers and construction trades, with practical controls for MIG/GMAW, stick/SMAW and limited TIG/GTAW applications on galvanised components. For any structural or load-bearing work, welding procedures and acceptance criteria should align with AS/NZS 1554 and site-specific SWMS/JSA requirements.

What skill level is required for welding galvanised steel on site?

Intermediate — Estimated time: 1–4 hours depending on access, quantity of welds, surface prep and ventilation setup

What tools are essential for welding galvanised steel safely on site?

MIG/GMAW welder rated for site use, ideally 180–250 A with stable output
Stick/SMAW welder or engine drive welder for remote/site work
TIG/GTAW welder only where required for controlled thin-section work
4" or 5" angle grinder with flap discs, grinding discs and wire cup brush
Local exhaust ventilation or portable fume extractor with suitable filtration
PAPR welding helmet or respirator-compatible auto-darkening helmet meeting AS/NZS 1338.1
Respiratory protection selected to suit zinc fume exposure and site risk assessment
G-clamps, magnets, vice grips and fit-up tools
Infrared thermometer or temperature crayons for managing preheat/interpass where required
Fire extinguisher minimum suitable for hot work area, plus fire blanket where required
Measuring tape, square, scriber, soapstone and marking tools
Chipping hammer and stainless or dedicated steel wire brush for slag/spatter removal

Materials Required

Galvanised steel components to be joined
Mild steel filler wire such as ER70S-6 for MIG on most galvanised mild steel after coating removal
Stick electrodes such as E6013 or E7018 depending on application and procedure
Shielding gas for MIG, commonly Argon/CO₂ mix such as 75/25 or similar
Anti-spatter spray where appropriate
Solvent cleaner/degreaser suitable for weld prep
Clean rags
Zinc-rich cold galvanising compound for post-weld corrosion repair
Marking paint or tags for hot work exclusion zones if required by site
Replacement grinding consumables and extraction filters as required

Safety Requirements

Welding helmet with compliant lens protection to AS/NZS 1338.1
Safety glasses and face protection to AS/NZS 1337.1
Leather welding gloves, FR jacket/apron and non-synthetic long sleeves/trousers
Steel cap boots and hearing protection
Effective fume extraction and ventilation — galvanised steel welding must not be done in stagnant or enclosed atmospheres without engineered controls
Respiratory protection selected under site risk controls; galvanised welding fumes require higher attention than plain mild steel
Hot work permit, SWMS/JSA and isolation of nearby combustibles
Fire extinguisher, fire watch/spotter and post-work fire check
UV/arc flash screening to protect bystanders
For confined spaces, follow confined space entry procedures and atmospheric testing requirements
For structural or load-bearing welds, comply with AS/NZS 1554 and relevant WPS/PQR requirements

Step-by-Step Guide

Step 1: Assess the job, coating condition and site risks

1️⃣ Identify the material and work scope

Confirm the item is hot-dip galvanised mild steel and determine whether the weld is non-structural, architectural, or load-bearing. Check drawing notes, project specifications and any nominated welding procedure.

Inspect the galvanised coating thickness, contamination, paint, oil and access constraints. Heavy galvanising generally produces more fumes and more weld contamination if not removed properly.

For structural work, confirm the applicable procedure under AS/NZS 1554 and whether repair/rework must be signed off by a qualified supervisor or welding coordinator.

Step 2: Establish mandatory hot work and fume controls

2️⃣ Set up the site safely before striking an arc

Implement the site hot work permit and complete the relevant SWMS/JSA. Remove combustibles, establish exclusion zones and ensure a suitable extinguisher is immediately available.

Set up portable fume extraction close to the source without disturbing shielding gas. If working outdoors, position yourself upwind and avoid welding in pockets where fumes collect, such as between panels, inside fence returns or against walls.

Where natural ventilation is poor, do not rely on “open air” assumptions alone. Use mechanical extraction or reschedule the weld to a controlled area. Zinc oxide fume exposure can occur rapidly on short welds if prep and extraction are poor.

⚠️ Safety

Wear an auto-darkening welding helmet (AS/NZS 1338.1), leather gloves and FR clothing
Use respiratory protection appropriate to the task and site controls
Protect bystanders from arc flash and fume drift
Assign a fire spotter where required and complete post-hot-work fire checks

Step 3: Remove galvanising from the weld zone

3️⃣ Grind back the zinc coating before welding

Mechanically remove the galvanised coating from both sides of the joint wherever possible. As a practical guide, grind back at least 25–50 mm from the weld line, and further on heavier coatings or where porosity has previously been an issue.

Remove zinc from:

The weld face side
The root side where accessible
The immediate tack weld locations
Earth clamp contact area

Use a grinder with a flap disc rather than only a wire brush. A wire brush alone often polishes the coating without fully removing it. You need bright, clean parent metal in the fusion zone.

Avoid excessive gouging or thinning the base material. The aim is to remove coating and contamination while maintaining joint geometry.

💡 Pro tip: If you can still see a mottled silver zinc finish in the fusion path, you have not prepped enough.

Step 4: Prepare the joint and fit-up correctly

4️⃣ Control fit-up to reduce blow-outs and contamination

Prepare the joint to suit thickness and process. Tight fit-up can trap zinc vapours and create porosity, worm tracks and excessive spatter. In some site applications, a slight root opening helps vent vapours and improves penetration control.

Typical guidance:

Thin galvanised sections under 3 mm: favour small fillets, controlled travel speed and minimal heat input
3–6 mm galvanised mild steel: MIG or stick both suitable with good prep
Over 6 mm: use proper bevel prep where required and verify procedure for structural work

Clamp securely and place tacks on fully cleaned steel. If tack welds porosity immediately, stop and grind cleaner/further back before continuing.

Step 5: Select the best welding process and consumables

5️⃣ Choose a process that suits site conditions

For most on-site galvanised steel work:

MIG/GMAW is preferred for productivity on fencing, brackets, frames and light fabrication
Stick/SMAW is often better in windy conditions and remote work
TIG/GTAW is generally less practical on galvanised steel on site due to contamination sensitivity and prep demands

Recommended consumables:

MIG wire: ER70S-6 on cleaned galvanised mild steel
Gas: Argon/CO₂ mix, typically 75/25
Stick electrodes: E6013 for general-purpose site work, E7018 where procedure strength/toughness requirements apply

Suggested starting settings only, to be adjusted for joint, position and machine:

MIG on 3 mm mild steel after zinc removal: 18–20 V, 4.5–6.0 m/min wire speed, 10–15 L/min gas flow
MIG on 5 mm mild steel after zinc removal: 20–23 V, 6.0–8.0 m/min wire speed, 12–16 L/min gas flow
Stick on 3–5 mm steel with E6013 2.5–3.2 mm rod: approximately 80–130 A
Stick on 5–8 mm steel with E7018 3.2 mm rod: approximately 110–140 A

If extraction airflow disrupts shielding gas on MIG, adjust extractor position rather than simply increasing gas flow excessively.

Step 6: Run test welds and confirm fume behaviour

6️⃣ Trial first before production welding

Before welding in full, run a short test on offcut or a non-critical section. Check for:

Porosity
Excessive spatter
Pinholes
Worm tracking
Arc instability
Fume volume and direction

If the weld is boiling, dirty or porous, the most common issue is still residual galvanising in or behind the joint. Stop, grind further back and retest.

Monitor your breathing zone. If fumes are passing through the helmet area, reposition yourself, the workpiece or the extraction nozzle.

Step 7: Weld using controlled technique

7️⃣ Use a smooth, deliberate technique to minimise zinc contamination

For MIG/GMAW, use a steady travel speed and maintain a short, stable arc. A slight push technique is commonly used on clean mild steel, but on galvanised material after prep, technique should prioritise visibility, gas coverage and control of residual contamination rather than fixed habit.

For stick/SMAW, keep arc length tight and avoid whipping excessively. Restart only after cleaning slag and checking for porosity.

Practical points:

Use shorter weld runs if fume build-up is occurring
Pause between runs to allow extraction to clear the plume
Clean between passes thoroughly
If zinc is present on the back side, expect more outgassing and watch for root contamination

On thin galvanised sections, avoid overheating and burn-through. On heavier work, ensure enough heat input for fusion once the zinc has been removed.

Step 8: Inspect, clean and repair defects immediately

8️⃣ Do not paint over bad welds

Visually inspect the weld for:

Surface porosity
Undercut
Lack of fusion
Excessive convexity
Cracking
Slag inclusions on stick welds

Any porous or contaminated weld sections must be ground out and rewelded on properly cleaned steel. Do not assume the zinc-rich touch-up coating will “seal” a defective weld.

For structural work, inspection and acceptance must follow the relevant code, project specification and AS/NZS 1554 category requirements.

Step 9: Restore corrosion protection after welding

9️⃣ Recoat the affected area correctly

After the weld has cooled and passed inspection, remove spatter, clean the surrounding steel and apply an approved zinc-rich cold galvanising compound or specified corrosion protection system.

Follow the product’s dry film thickness and surface prep instructions. On exposed outdoor work such as fencing, gates and structural supports, proper post-weld coating repair is essential because the original galvanising has been destroyed in the heat-affected zone.

If the project specifies duplex coating, paint system compatibility must be confirmed.

Step 10: Complete final safety checks and documentation

🔟 Close out the hot work properly

Inspect the work area for smouldering materials, hidden ignition points and retained heat. Complete the fire watch period required by site rules or permit conditions.

Dispose of grinding dust and consumables appropriately. Record any structural repairs, coating repairs and inspection outcomes as required by the project QA system.

If multiple workers are repeating the task, review whether the extraction setup and prep method were adequate or need improvement before continuing.

Common Mistakes to Avoid

1.Welding straight over galvanising and assuming “the arc will burn through it” — this causes heavy fumes, porosity and poor weld quality.
2.Relying on outdoor air alone without positioning for airflow or using extraction — on-site exposure can still be significant, especially near walls, corners or inside framed sections.
3.Using a wire brush only instead of fully grinding back the zinc coating to bright steel.
4.Poor earth clamp contact on galvanised or dirty surfaces, leading to unstable arc starts and overheating.
5.Skipping post-weld coating repair, leaving bare heat-affected areas to corrode rapidly.

Pro Tips

💡 Grind back more galvanising than you think you need. Most weld issues on galvanised steel come from insufficient prep, not machine settings.
💡 Position extraction to capture the plume at source without stripping shielding gas away from the arc.
💡 For repetitive fence or bracket work, set up a dedicated prep station so every joint is cleaned consistently before fit-up.
💡 If a weld starts “boiling” or throwing unusual spatter, stop immediately and clean the joint again rather than trying to weld through contamination.
💡 Keep a dedicated can of zinc-rich touch-up coating in the site kit so corrosion protection is restored the same day.

Recommended Tools

Speedglas G5 series PAPR welding helmet — strong option for galvanised welding where respiratory protection and comfort matter
Cigweld or Weldclass fume extraction unit — useful for mobile source capture on fabrication and installation work
9" or 125 mm flap discs (zirconia) — effective for removing galvanising cleanly without excessive gouging
Lincoln, Miller or Kemppi 180–250 A MIG welder — suitable output range for general galvanised site fabrication
BOC Argoshield-style shielding gas — reliable mixed gas option for MIG on cleaned galvanised mild steel

For welders, extractors or engine drives over $1,000, many trades look at equipment finance options through Local Knowledge Finance to preserve cash flow on site setup.

Frequently asked questions

Do you need to remove galvanising before welding?
Yes, galvanising must be ground back at least 50mm either side of the weld line before welding. Leaving zinc coating in place causes excessive zinc oxide fume generation, weld porosity, inclusions and reduced weld integrity, increasing both health risk and the likelihood of structural weld failure.
What PPE is required for welding galvanised steel in Australia?
A PAPR (powered air-purifying respirator) welding helmet meeting AS/NZS 1716, along with flame-resistant clothing, welding gloves and local exhaust ventilation, is the minimum PPE standard. Standard disposable P2 masks do not provide adequate protection against zinc oxide fume inhalation.
Can you weld galvanised steel without ventilation?
No, welding galvanised steel without mechanical ventilation or local exhaust extraction is unsafe and breaches SafeWork Australia's model Code of Practice for welding processes. Even outdoor sites require positioning for cross-airflow or portable fume extraction, particularly in corners, trenches or partially enclosed framed structures.
What welding process is best for galvanised steel on site?
MIG/GMAW welding, typically using a 180-250 amp site-rated machine, is the most common process for galvanised steel on site due to controllable heat input and travel speed. Stick/SMAW suits rougher field conditions, while TIG/GTAW is reserved for thin-gauge, high-quality joints.
What happens if you inhale zinc oxide fumes from welding?
Inhaling zinc oxide fumes causes metal fume fever, with flu-like symptoms including fever, chills, nausea and muscle aches appearing 4-12 hours after exposure. Symptoms usually resolve within 24-48 hours, but repeated exposure without respiratory protection increases long-term respiratory health risks.
What hot work permit requirements apply to welding galvanised steel on site?
A hot work permit is typically required before welding galvanised steel on construction sites, covering fire watch, fume extraction checks and clearance of combustible materials. Requirements are set by the site's WHS management plan in line with SafeWork Australia's hot work guidance.

Written by Welder, the Welding & Fabrication specialist at VIC.Tools.