How to TIG Weld Aluminium
Learn how to TIG weld aluminium using AC current, argon shielding gas, and correct filler wire. Step-by-step Australian trade guide for faultless weld beads.
Quick answer
To TIG weld aluminium, use an AC-capable TIG welder set to pure argon shielding gas at 7 to 12 litres per minute. Clean the joint using acetone and a dedicated stainless steel brush to break down the surface oxide. Use zirconiated or lanthanated tungsten and add 4043 or 5356 filler.
- Skill level
- Advanced
- Time
- 2-4 hours practice
- Trade
- Welding & Fabrication
- Updated
- 28 November 2026
Tools you will need
- Kemppi MasterTig 235ACDC or Cigweld WeldSkill 200AC/DC - Inverter TIG Welder
- BOC Pure Shield Argon - High-Purity Argon Shielding Gas Cylinder and Regulator
- CK Worldwide 17V Flex-Head - TIG Torch with Foot Control Pedal
- WIA or Cigweld 1.6mm/2.4mm Zirconiated (White) or Lanthanated (Gold) - Tungsten Electrodes
- Cigweld Autocraft AL4043 / AL5356 - Aluminium TIG Filler Rods
- Josco 0.30mm Stainless Steel - Dedicated Hand Wire Brush
- Speedglas 9100XX - Auto-Darkening Welding Helmet with Shade 10-13
- Diggers Acetone - Hydrocarbon Degreaser
What is TIG welding aluminium and why is it an advanced skill?
Set up and TIG weld aluminium including AC settings, tungsten selection, filler rod, and cleaning techniques.
This guide walks you through every stage of the process, from preparation and tool selection right through to finishing. Whether you are tackling this project for the first time or looking to refine your technique, the steps below will help you achieve a professional result.
Skill Level: Advanced | Estimated Time: 2-4 hours practiceWhat essential preparations should you make before TIG welding aluminium?
Before picking up any tools, take a few minutes to prepare properly. Good preparation is the difference between a smooth project and a frustrating one.
What specific tools and materials are required for TIG welding aluminium in Australia?
Having the right tools makes every step faster, safer, and more accurate. Below is the complete tool list for this project. If you do not own a particular tool, consider whether hiring or purchasing makes more sense for your situation -- tools over $300 may be eligible for the EOFY instant asset write-off if used for income-producing purposes.
Step-by-Step Guide
Follow these steps in order. Each step builds on the previous one, so resist the temptation to skip ahead. Take your time with the early stages -- accurate preparation saves hours of correction later.
Step 1: Clean aluminium thoroughly: remove oxide with stainless steel brush then wipe with acetone
This is your foundation step. Getting this right sets the standard for everything that follows. Double-check all measurements and marks before committing to any cuts or fixings. If something does not look right at this stage, it is far easier to adjust now than after you have progressed further.
Step 2: Set welder to AC (alternating current) for aluminium
With your initial preparation complete, this step moves you into the main construction phase. Ensure all your materials are within reach and your work area is clear of obstructions. Maintain consistent technique throughout to achieve uniform results.
Step 3: Select tungsten: pure (green) or zirconiated (white) for AC welding
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 4: Grind tungsten to a ball tip by briefly arcing on scrap
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 5: Set AC balance: 65-70% EN (cleaning), 30-35% EP (penetration)
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 6: Set frequency: higher frequency (80-120 Hz) for tighter arc
You are at the midpoint of the project. This is a good time to pause, check your progress against the plan, and verify everything is level, plumb, and square. Correcting small errors now prevents them from compounding through the remaining steps.
Step 7: Set gas flow: 12-18 L/min pure Argon
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 8: Use a foot pedal for amperage control during welding
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 9: Add filler rod by dipping into the leading edge of the puddle
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 10: Travel at a consistent speed watching the puddle not the arc
This final step brings the project together. Take your time here and focus on the finish quality. Step back and inspect your work from different angles. Small adjustments at this stage make a significant difference to the overall appearance and performance of the finished result.
Safety Notes
Safety is not optional. Australian workplace health and safety regulations apply to all construction work, including domestic projects. The notes below highlight specific hazards for this project.
Always have a first aid kit accessible at your work site. If you are working alone, let someone know where you are and what you are doing.
Pro Tips from the Trade
These tips come from years of hands-on experience. They represent the kind of knowledge that separates a good job from a great one.
Tip 1: AC cleaning action removes the oxide layer while welding. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 2: 4043 filler is easier to weld with, 5356 is stronger. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 3: Pre-heat thick aluminium to 100-150C to improve fusion. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 4: A foot pedal gives much better heat control than fixed amperage. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time.Common Mistakes to Avoid
Learning from other people's mistakes saves you time, money, and frustration. These are the most common errors seen in this type of project.
Mistake 1: Not cleaning the aluminium oxide layer before welding. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 2: Using DC instead of AC which cannot clean the oxide. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 3: Contaminating the tungsten by dipping it in the puddle. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 4: Using too much heat causing the aluminium to melt through suddenly. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time.Materials List
Below is the complete materials list. Quantities will vary based on your specific project dimensions. Always purchase 10-15% extra to account for cuts, waste, and any errors during construction. Check availability at your local supplier before starting the project.
When to Call a Professional
While this guide covers a advanced-level project that many competent DIYers can tackle, there are situations where professional help is the smarter choice:
Hiring a licensed professional for critical aspects of the work is not a sign of failure -- it is a sign of good judgement. The cost of getting it right the first time is always less than the cost of fixing it later.
Frequently asked questions
- Why do you need AC current to TIG weld aluminium?
- Alternating current is required for TIG welding aluminium because it alternates between electrode positive and electrode negative cycles. The positive cycle provides cathodic cleaning to scour off the heavy aluminium oxide layer, while the negative cycle delivers deep penetration into the base metal. DC welding cannot break down this refractory oxide surface.
- What is the difference between 4043 and 5356 aluminium filler wire?
- Aluminium 4043 filler contains 5% silicon, offering higher puddle fluidity, lower crack sensitivity, and a brighter finish on 6000-series alloys. In contrast, 5356 contains 5% magnesium, which provides higher shear strength and matches anodised colours better, making it the preferred wire for marine-grade 5000-series aluminium fabrication.
- What tungsten electrode is best for TIG welding aluminium?
- Zirconiated tungsten electrodes (white tip) or rare-earth lanthanated electrodes (gold tip) are best for AC aluminium TIG welding. Zirconiated retains a stable balled tip under high AC amperage, while 1.5% to 2% lanthanated maintains a micro-ball or modified point for tighter arc control on modern inverter welders.
- How should aluminium be prepared before TIG welding?
- Mechanically degrease the joint using acetone, then remove the aluminium oxide skin using a dedicated stainless steel wire brush. Never use wire brushes previously used on mild steel to avoid cross-contamination. Wipe the weld zone again with acetone immediately before striking an arc to eliminate surface hydrocarbons and moisture.
- What Australian standards regulate aluminium welding and safety?
- Aluminium structural welding in Australia is governed by AS/NZS 1665, which defines qualification, weld preparations, and inspection requirements. Workshop electrical and welding safety compliance must adhere to AS 1674.2, covering high-frequency arc stabilisation hazards, proper earthing, personal protective equipment, and mandatory eye protection conforming to AS/NZS 1338.1.
- What gas flow rate and shielding gas are used for aluminium TIG welding?
- Pure argon rated at 99.995% purity is the standard shielding gas, set to a flow rate between 7 and 12 litres per minute depending on ceramic cup size. For thick aluminium plate exceeding 6 millimetres, argon-helium mixtures can be utilised to boost heat input and increase weld penetration.