How to Use an Oxy-Acetylene Torch
Safely set up and use an oxy-acetylene torch for cutting, heating, brazing, and welding.
- Skill level
- Intermediate
- Time
- 1-2 hours practice
- Trade
- Welding & Fabrication
- Updated
- 28 November 2026
Tools you will need
- Oxy-acetylene outfit (bottles, regulators, hoses, torch)
- Cutting and welding tips
- Lighter (spark igniter)
- Safety glasses (shade 5)
- Gloves and leathers
What is an oxy-acetylene torch used for in Australian trades?
Safely set up and use an oxy-acetylene torch for cutting, heating, brazing, and welding.
This guide walks you through every stage of the process, from preparation and tool selection right through to finishing. Whether you are tackling this project for the first time or looking to refine your technique, the steps below will help you achieve a professional result.
Skill Level: Intermediate | Estimated Time: 1-2 hours practiceWhat essential safety checks are required before using an oxy-acetylene torch?
Before picking up any tools, take a few minutes to prepare properly. Good preparation is the difference between a smooth project and a frustrating one.
What specific tools and PPE are required for oxy-acetylene welding in Australia?
Having the right tools makes every step faster, safer, and more accurate. Below is the complete tool list for this project. If you do not own a particular tool, consider whether hiring or purchasing makes more sense for your situation -- tools over $300 may be eligible for the EOFY instant asset write-off if used for income-producing purposes.
Step-by-Step Guide
Follow these steps in order. Each step builds on the previous one, so resist the temptation to skip ahead. Take your time with the early stages -- accurate preparation saves hours of correction later.
Step 1: Check all connections for tightness and condition of hoses
This is your foundation step. Getting this right sets the standard for everything that follows. Double-check all measurements and marks before committing to any cuts or fixings. If something does not look right at this stage, it is far easier to adjust now than after you have progressed further.
Step 2: Open oxygen bottle valve fully then back off quarter turn
With your initial preparation complete, this step moves you into the main construction phase. Ensure all your materials are within reach and your work area is clear of obstructions. Maintain consistent technique throughout to achieve uniform results.
Step 3: Open acetylene bottle valve maximum 1.5 turns
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 4: Set regulators: cutting - oxy 250kPa, acet 70kPa
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 5: Purge each line separately before lighting
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 6: Light acetylene first, then add oxygen to achieve neutral flame
You are at the midpoint of the project. This is a good time to pause, check your progress against the plan, and verify everything is level, plumb, and square. Correcting small errors now prevents them from compounding through the remaining steps.
Step 7: Adjust to neutral flame: equal size inner cone, no acetylene feather
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 8: For cutting: preheat to cherry red, press oxygen lever to start cut
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 9: For heating: use a rosebud tip with a softer flame
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 10: For brazing: use neutral flame and bronze filler rod
Work methodically through this step, checking your progress as you go. Accuracy at each stage ensures the final result meets a professional standard. If you are unsure about any aspect, refer back to the measurements and specifications noted earlier.
Step 11: Shut down: close acetylene first, then oxygen at torch, then bottles
This final step brings the project together. Take your time here and focus on the finish quality. Step back and inspect your work from different angles. Small adjustments at this stage make a significant difference to the overall appearance and performance of the finished result.
Safety Notes
Safety is not optional. Australian workplace health and safety regulations apply to all construction work, including domestic projects. The notes below highlight specific hazards for this project.
Always have a first aid kit accessible at your work site. If you are working alone, let someone know where you are and what you are doing.
Pro Tips from the Trade
These tips come from years of hands-on experience. They represent the kind of knowledge that separates a good job from a great one.
Tip 1: A neutral flame has a clearly defined inner cone. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 2: The cutting oxygen lever does the cutting - the preheat just gets it started. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 3: For long cuts: use a straight edge as a guide. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time. Tip 4: Oxy cutting steel up to 300mm thick is routine. This may seem like a small detail, but experienced tradespeople consistently use this technique to deliver a better result in less time.Common Mistakes to Avoid
Learning from other people's mistakes saves you time, money, and frustration. These are the most common errors seen in this type of project.
Mistake 1: Using oil or grease on regulators (oxygen causes explosive reaction). This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 2: Not purging lines before lighting causing popping. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 3: Opening acetylene valve more than 1.5 turns. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time. Mistake 4: Not fitting flashback arrestors on both lines. This is one of the most frequent problems encountered. It can result in wasted materials, poor structural integrity, or the need to redo significant portions of the work. Take the time to get it right the first time.Materials List
Below is the complete materials list. Quantities will vary based on your specific project dimensions. Always purchase 10-15% extra to account for cuts, waste, and any errors during construction. Check availability at your local supplier before starting the project.
When to Call a Professional
While this guide covers a intermediate-level project that many competent DIYers can tackle, there are situations where professional help is the smarter choice:
Hiring a licensed professional for critical aspects of the work is not a sign of failure -- it is a sign of good judgement. The cost of getting it right the first time is always less than the cost of fixing it later.
Frequently asked questions
- What tools do I need for use an oxy-acetylene torch?
- You will need: Oxy-acetylene outfit (bottles, regulators, hoses, torch), Cutting and welding tips, Lighter (spark igniter), Safety glasses (shade 5), Gloves and leathers.
- How long does it take to use an oxy-acetylene torch?
- Expect approximately 1-2 hours practice for this project.
- What safety precautions should I take?
- NEVER use oil or grease near oxygen fittings - explosion risk. Open acetylene bottle maximum 1.5 turns (quick closure in emergency). Test for leaks with soapy water, never a flame. Keep fire extinguisher within reach at all times. Flashback arrestors must be fitted to both lines.
- What are the best tips for success?
- A neutral flame has a clearly defined inner cone. The cutting oxygen lever does the cutting - the preheat just gets it started. For long cuts: use a straight edge as a guide. Oxy cutting steel up to 300mm thick is routine.
- What mistakes should I avoid?
- Using oil or grease on regulators (oxygen causes explosive reaction). Not purging lines before lighting causing popping. Opening acetylene valve more than 1.5 turns. Not fitting flashback arrestors on both lines.
- What is the Australian standard for flashback arrestors on oxy-acetylene equipment?
- The Australian standard for flashback arrestors is AS 4267-1995 'Gas welding and cutting equipment - Flashback arrestors'. This standard mandates that flashback arrestors must be fitted to both the oxygen and acetylene lines at the torch end or regulator outlet to prevent dangerous flashbacks into the gas supply system. Always ensure your equipment complies with this standard for maximum safety.
- What shade of safety glasses is required for oxy-acetylene work in Australia?
- For oxy-acetylene cutting and welding, AS/NZS 1338.1:2012 'Filters for eye protectors' specifies a minimum shade of 5. However, for heavier cutting or welding operations, a higher shade, such as 6 or 7, may be more appropriate to protect against intense radiant energy. Always select the correct shade based on the intensity of the work being performed.
- Can I claim oxy-acetylene equipment as an instant asset write-off in Australia?
- Yes, if you are a small business or sole trader, oxy-acetylene equipment purchased for income-producing purposes may be eligible for the instant asset write-off. According to the Australian Taxation Office (ATO), for the 2023-24 income year, the threshold is $20,000 ex GST per asset. Always consult the latest ATO guidelines or a tax professional for current eligibility criteria.
- What are the legal requirements for storing oxy-acetylene cylinders in Australia?
- SafeWork Australia guidelines, adopted by state and territory regulators, stipulate that oxygen and acetylene cylinders must be stored separately, ideally by a fire-resistant barrier or a minimum distance of 3 metres. Cylinders must be secured upright to prevent falling and protected from heat sources, ignition, and unauthorised access. Proper ventilation is also crucial to prevent gas accumulation.
Written by Welder, the Welding & Fabrication specialist at VIC.Tools.